MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Eastman Kelvx 201 Resin  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Kelvx resin provides long-term durability and temperature resistance for outdoor applications. Sheet made with Kelvx resin expands design options, while providing manufacturing flexibility, impact resistance, ease of fabrication, and superior thermoforming characteristics - all of which can yield product differentiation, cost savings and total satisfaction for both the converter and the end customer.
The material failed to discharge under a Static Decay Rate test ASTM D4470.

Applications/Uses

  • Architectural glazing
  • Signs
  • Key Attributes

  • Approximately 20 times the impact strength of impact
  • Good chemical resistance
  • Available from plastic sheet distributors globally
  • Thermoforms without pre-drying
  • UV protection
  • Can be painted, printed, or vinyl decorated
  • Excellent thermoforming characteristics
  • Thermoforms at lower temperatures than acrylic or polycarbonate
  • Up to 50% faster thermoforming cycle times
  • Vendors:
    Available Properties
    • Specific Gravity, ASTM D792
    • Water Absorption, ASTM D570, 24h Immersion
    • Thickness
    • Tensile Strength at Break, ASTM D638
    • Tensile Strength, Yield, ASTM D638
    • Tensile Modulus, ASTM D638
    • Flexural Strength, ASTM D790
    • Flexural Modulus, ASTM D790
    • Izod Impact, Notched, ASTM D256
    • Izod Impact, Notched, ASTM D256
    • Izod Impact, Unnotched, ASTM D4812
    • Izod Impact, Unnotched, ASTM D4812
    • Puncture Energy, ASTM D3763, Puncture Resistance @Max Load, 23°C
    • Puncture Energy, ASTM D3763, Puncture Resistance @Max Load, -10°C
    • Puncture Energy, ASTM D3763, Puncture Resistance @Max Load, -30°C
    • Volume Resistivity, ASTM D257
    • Surface Resistivity per Square, ASTM D257
    • Arc Resistance, ASTM D495
    • CTE, linear, ASTM D696
    • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
    • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
    • Vicat Softening Point, ASTM D1525
    • Flammability, UL94
    • Haze, ASTM D1003
    • Gloss, ASTM D2457, at 60°
    • Yellow Index, ASTM D2244
    • Transmission, Visible, ASTM D1003, Total Transmittance
    • Processing Temperature, Thermoforming Soak Temperature
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Eastman Chemical Company

    Category Notes
    Plastic

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.