MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond Polymer Adhesive EP21ANHT is a two component room temperature curing adhesive, sealant and coating that combines high thermal conductivity and electrical insulation properties, along with elevated temperature resistance. It has a forgiving one to one mix ratio by weight or volume. Although the system cures at room temperature, its physical properties are optimized by a post cure at 150°F for 2-3 hours. EP21ANHT adheres well to a wide variety of substrates including metals glass and many plastics. Its tensile shear strength exceeds 1,100 psi, enabling it to be used in many applications where high strength bonds are required. Other features include superior dimensional stability and a long working life. EP21ANHT offers good resistance to a wide range of chemicals including water, oil, fuels, and various solvents over the temperature range of -60°F to +400°F. The color of Part A is light gray; Part B is gray in color. EP21ANHT is widely used in electronic, electrooptical and related industries where excellent heat transfer and electrical insulation are required.

Product Advantages:

  • Convenient mixing: non-critical equal weight or volume ratio.
  • Long working life.
  • Easy application: contact pressure only required for cure; adhesive spreads evenly.
  • Low coefficient of expansion, low shrinkage, superb dimensional stability.
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures as required.
  • High bonding strength to a wide variety of substrates.
  • Good durability, thermal shock and chemical resistance.
  • Great thermal conductivity; excellent electrical insulation properties.

Information provided by MasterBond®

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength at Break
  • Tensile Modulus
  • Shear Strength, Al/Al, tensile
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Pot Life, 100 gram mass
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.