Hifax polypropylene resins based on the Catalloy process from LyondellBasell are used by customers in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable) and also automotive industries through both our resins and our well-known Hifax polypropylene compounds. Hifax is proven to provide customers with good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax TYC 258P 9B9 BLACK is a 30% talc reinforced, impact modified, UV stabilized polypropylene copolymer resin for injection molding. It combines excellent flowability with low coefficient of linear thermal expansion and very good processability. This grade is typically used for molding of large complex parts that require good dimensional stability. Applications: Automotive Parts, Exterior Automotive Applications. |