Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature range, low moisture absorption, excellent chemical resistance and excellent electrical properties. Features: Fast Molding Cycle; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength; Hot Water Moldability; Low Moisture Absorption; Lubricated Uses: Abrasive Cleaning Material; Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Thick-walled Parts; Valves/Valve Parts Injection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding. Automotive Specifications ASTM D6779 PA102G45; TYCO 100-1632 Color: BK-324 Black Information provided by Solvay Specialty Polymers. |