Veradel® PESU was formerly marketed as Gafone™ PESU Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability as well as resistance to steam, hot water and mineral acids. Other desirable properties include thermal stability, creep resistance, and inherent flame resistance. Veradel® 3200 is a low melt flow grade that can be processed by extrusion or injection molding. It is FDA compliant and approved for direct food contact. Veradel® 3300 is a medium melt flow, general purpose grade for injection molding. Veradel® 3400 is a high melt flow grade designed for molding of parts with thin walls or long flow lengths. Acid Resistant; Chemical Resistant; Creep Resistant; Flame Retardant; General Purpose; Good Adhesion; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight; Medium Rigidity Uses: Food Service Applications; General Purpose Processing: Injection Molding Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Information provided by Solvay Specialty Polymers. |