Features: Good Chemical Resistance; Good Dimensional Stability; Heat Stabilized; High Heat Resistance; Impact Modified
Uses: Appliance Components; Appliances; Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bearings; Connectors; Fuel Lines; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement
Injection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.
Automotive Specifications ASTM D4000 PA123 G25; ASTM D4000 PPA0111 G25 KD160 KN075 LD002 PN080 YI250; ASTM D6779 PA123G25; ISO 1874 PA6T/6I/66-HI, MH, 12-080, GF25
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic