MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
SABIC Lexan® FR735A Polycarbonate Film, Flame Retardant  (Unverified Data**)
Categories: Polymer; Film; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensional stability at high temperatures and a high flammability rating, making it good for applications such as power supply insulation, disc drive insulation, bus-bar insulation, TV/monitor insulation, PC board insulation, business equipment insulation and has insulation and EMI/RFI shielding when laminated with metal foil.

Information provided by SABIC Innovative Plastics

Key Words: PC
Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570, 24 hrs
  • Surface Tension, Dyne Pens, 1st surface; units: Dyne
  • Surface Tension, Dyne Pens, 2nd surface; units: Dyne
  • Tensile Strength, Ultimate, ASTM D882
  • Tensile Strength, Yield, ASTM D882
  • Elongation at Break, ASTM D882
  • Tensile Modulus, ASTM D882
  • Flex Crack Resistance, ASTM D2176-69, Folds; MIT Test; Double
  • Flex Crack Resistance, ASTM D2176-69, Folds; MIT Test; Double
  • Gardner Impact, ASTM D3029
  • Impact Test, ASTM D3763, Puncture Resistance, Dynatup
  • Tear Strength, ASTM D1922, propagation
  • Tear Strength, ASTM D1004, initiation
  • Volume Resistivity, ASTM D257
  • Surface Resistivity per Square, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149-97a Method A, in oil, short time. 0.25mm
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495, Tungsten
  • CTE, linear, ASTM E831
  • Specific Heat Capacity, ASTM E1269
  • Thermal Conductivity, ASTM D5470
  • Deflection Temperature at 1.8 MPa (264 psi), TMA
  • Vicat Softening Point, ASTM 1525-00 modified
  • Brittleness Temperature, ASTM D746
  • Glass Transition Temp, Tg, ASTM D3417/D3418
  • Flammability, UL94
  • Flammability, UL94
  • Shrinkage, ASTM D1204
  • Gloss, ASTM D523-60, over Flat Black min/max @ 60º
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.