Hifax polypropylene resins based on the Catalloy process from LyondellBasell are used by customers in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable) and also automotive industries through both our resins and our well-known Hifax polypropylene compounds. Hifax is proven to provide customers with good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax EKG 2037X BLACK is a mixed filler grade, elastomer modified PP, with glass fiber reinforcing and talc filling, high stiffness and good dimensional stability. The product is available in black color, pellet form. |