Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.125 in (3 mm). Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength; Low Moisture Absorption Uses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; Fuel Lines; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Oil/Gas Applications; Power/Other Tools; Thick-walled Parts; Valves/Valve Parts Injection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding. Automotive Specifications ASTM D4000 PA121 G35 Color: BK324 Black; ASTM D4000 PA121 G35 Color: NT Natural; ASTM D4000 PPA0111 G33 GB145 KD200 KN090 PN080 YI265 Color: BK324 Black; ASTM D4000 PPA0111 G33 GB145 KD200 KN090 PN080 YI265 Color: NT Natural; ASTM D6779 PA121G35; BOSCH N28 BN05-OX1 BN0510-GF35-3Anf01SO Color: NT Natural; BOSCH N28 BN05-OX1 BN0510-GF35-3Asw01SO Color: BK324 Black; DELPHI M-6071 Color: NT Natural; FORD WSK-M4D843-A2 Color: BK324 Black; FORD WSK-M4D843-A2 Color: NT Natural; ISO 1874 PA6T/6I/66, MH, 12-120, GF33 Color: BK324 Black; ISO 1874 PA6T/6I/66, MH, 12-120, GF33 Color: NT Natural; SIEMENS S219536 Color: NT Natural Information provided by Solvay Specialty Polymers. |