MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
LyondellBasell Lupolen 1800U Polyethylene  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Lupolen 1800U is a low density polyethylene resin used in various processing methods such as injection molding and compounding. It exhibits very high flowability and a very good balance of softness and toughness, dimensional stability and good processing. Lupolen 1800U is delivered in pellet form and is not additivated. It is used in a wide range of injection molding applications such as thin-wall packaging (TWIM) and housewares. Lupolen 1800U is also used in the area of compounding for color and additive batches and as a viscosity modifier. Customers have reported that the high melt flow rate (MFR) of Lupolen 1800U enables very good dispersion and homogenization at high loads with pigments and additives. Lupolen 1800U is not intended for use in medical and pharmaceutical applications. Applications :Caps & Closures, Color Concentrates, Housewares, Sports, Leisure & Toys

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Environmental Stress Crack Resistance, ASTM D1693, cond. B, 10% Arkopal N100
  • Melt Flow, ISO 1133-1
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Yield, ISO 527-1,-2
  • Elongation at Break, ISO 8986-2
  • Tensile Modulus, ISO 527-1,-2
  • Melting Point, ISO 3146
  • Vicat Softening Point, ISO 306, A50N
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell (former Equistar)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.