MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Polymer System EP37-3FLFAN is a two component system for high performance potting, bonding, sealing and coating that is formulated to cure at room temperature or more rapidly at elevated temperatures. It has a convenient one to one mix ratio by weight or volume. It has an unusual blend of properties including exceptionally high thermal conductivity, excellent electrical insulation properties, good physical strength and a high degree of flexibility. This system forms tough bonds that are resistant to shock, impact and thermal cycling as well as chemicals including water, oil and many solvents. EP37-3FLFAN has low viscosity with excellent flow characteristics making it ideal as a thermally conductive potting epoxy. It is cryogenically serviceable over the wide temperature range of 4K to 250°F. Part A is light gray and Part B is gray in color. Master Bond EP37-3FLFAN is widely used in the electronic, electrical, computer, metalworking, aerospace and chemical industries where electrical insulation and good heat transfer are required. The attractiveness of EP37-3FLFAN lies in the fact that this thermally conductive system retains a high level of flexibility while having the desirable physical characteristics inherent in epoxies.

Product Advantages:

  • Convenient mixing: easy-to-use, non-critical one to one mix ratio by weight or volume.
  • Long working life; cures readily at room temperature and can be accelerated by heat.
  • Good thermal conductivity with excellent electrical insulation properties.
  • High bond strength to a wide variety of substrates; very good adhesive properties.
  • Low viscosity with excellent flowability; ideal for potting and casting.
  • Outstanding flexibility; resists rigorous thermal cycling, mechanical and thermal shocks.
  • Good overall physical strength properties and chemical resistance.
  • Cryogenically serviceable down to 4K.

Information provided by MasterBond®

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength at Break
  • Shear Strength, Bond, Al to Al
  • Peel Strength, T-peel, Al/Al
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Pot Life, 100 gram batch
  • Shelf Life, in original unopened container
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.