MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Syensqo (Solvay Specialty Polymers) KetaSpire® KT-880 CF PEEK  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: KetaSpire® KT-880 CF40 is a 40% chopped carbon fiber-reinforced polyetheretherketone (PEEK) supplied in a natural-colored, ultra-fine powder form. The carbon fiber content in the formulation is designed to provide maximum strength and stiffness properties in a filled PEEK compound. The resin enjoys all the key performance attributes for which PEEK is known including resistance to harsh chemical environments, high heat resistance (both short and long term), along with excellent fatigue resistance. This resin is a high flowing/low viscosity grade and is ideally suited for use in injection molding fabrication. It can be melt processed using standard thermoplastic melt processing equipment. Potential application areas for KT880 CF40 include uses in the aerospace industry and some other transportation applications where maximum mechanical properties are desired while maintaining a low specific gravity. Semiconductor fabrication is another industrial area of possible use for this resin as are the chemical processing, oil and gas, and health care industries

Availability:

  • Africa & Middle East
  • Asia Pacific
  • Europe
  • Latin America
  • North America
Filler/Reinforcement: Glass Fiber, 35% Filler by Weight

Features:

  • Autoclave Sterilizable
  • E-beam Sterilizable
  • Ethylene Oxide Sterilizable
  • Fatigue Resistant
  • Flame Retardant
  • Good Chemical Resistance
  • Good Dimensional Stability
  • Good Sterilizabiltiy
  • High Flow
  • High Heat Resistance
  • High Stiffness
  • High Strength
  • Radiation (Gamma) Resistant
  • Radiation Sterilizable
  • Radiotranslucent
  • Steam Resistant
  • Steam Sterilizable
Uses:
  • Aerospace Applications
  • Connectors
  • Dental Application
  • Electrical/Electronic Applications
  • Film
  • Hospital Goods
  • Industrial Applications
  • Medical Devices
  • Medical/Healthcare
  • Oil/Gas Applications
  • Pump Parts
  • Seals
  • Surgical Instruments
Forms: Pellets

Processing Method:

  • Injection Molding
  • Machining
  • Profile Extrusion

Information provided by Solvay

Vendors:
Available Properties
  • Density, ASTM D792
  • Viscosity, ASTM D3835, 1000 sec-1
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Flexural Strain at Break, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.