Torlon® 4200 has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep, and chemicals.- High Flow: Torlon® 420O EXT
Key Attributes: Chemical Resistant; Creep Resistant; Ductile; Flame Retardant; Good Electrical Properties; High Heat Resistance; High Temperature Strength; Ultra High Impact Resistance; Wear Resistant
Applications: Electrical/Electronic Applications; Machine/Mechanical Parts; Semiconductor Molding Compounds