MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Atom Adhesives AA-BOND F113 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-BOND F113 is an Optically Clear, low viscosity , High impact epoxy adhesives developed for bonding and small volume potting of plastic or glass optical fibers, lenses and prisms, LED displays, and other optical components. AA-BOND F113 is recommended for laminating, bonding, and sealing applications where excellent wetting, good pot life and improved impact strength properties are required. AA-BOND F113 is two parts adhesive easily mixed and cured at room temperature and develops strong bond to glass and glass fibers, ceramics, many metals and most rigid plastics. AA-BOND F113 bonds offer resistance to mechanical impact and thermal shock, and is also resistant to weather, water, gases and vapors, petroleum products, and mild acids and alkalis.

Appearance: Clear

Cure Type: Heat cure or Room Temperature

Benefits:

  • Low viscosity
  • Thermal shock and impact resistant
  • Low stress connections
Mix Ratio by weight: 100:30/Resin:Hardener

Typical Application: Fiber optic assembly, multimode and single mode connectors, small potting and sealing applications

Information provided by Atom Adhesives

Vendors:
Available Properties
  • Specific Gravity, uncured
  • Water Absorption at Saturation, cured
  • Viscosity, uncured
  • Hardness, Shore D
  • Adhesive Bond Strength, Lap shear, alum to alum
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Refractive Index, cured
  • Transmission, Visible, cured
  • Cure Time
  • Cure Time
  • Pot Life, uncured
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.