Available Properties |
---|
- Density, ASTM D792
- Water Absorption, ISO 62-1, 23°C/24hrs
- Water Absorption, SABIC method, 23°C/24hrs
- Moisture Absorption, ISO 62, 23°C / 50% RH
- Linear Mold Shrinkage, Flow, ASTM D955
- Linear Mold Shrinkage, Transverse, ASTM D955
- Tensile Strength at Break, ASTM D638, 5 mm/min
- Tensile Strength at Break, ISO 527, 5 mm/min
- Elongation at Break, ISO 527, 5 mm/min
- Elongation at Break, ASTM D638, 5 mm/min
- Tensile Modulus, ISO 527, 1mm/min
- Tensile Modulus, ASTM D638, 5 mm/min
- Flexural Strength, ASTM D790, brk, 1.3 mm/min, 50 mm span
- Flexural Strength, ISO 178, 2 mm/min; break
- Flexural Yield Strength, ASTM D790, 1.3 mm/min, 50 mm span
- Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
- Flexural Modulus, ISO 178, 2 mm/min
- Izod Impact, Notched, ASTM D256
- Izod Impact, Unnotched, ASTM D4812
- Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
- Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*4
- Charpy Impact Unnotched, ISO R179
- Surface Resistance, ASTM D257
- Dielectric Constant, ASTM ES 7-83
- Dielectric Strength, ASTM D149, in oil
- Dissipation Factor, ASTM ES 7-83
- Comparative Tracking Index, IEC 60112
- Comparative Tracking Index, UL 746A
- Hot Wire Ignition, HWI, UL 746A
- Hot Wire Ignition, HWI, UL 746A
- Hot Wire Ignition, HWI, UL 746A
- High Amp Arc Ignition, HAI, UL 746A
- CTE, linear, Parallel to Flow, ASTM E831
- CTE, linear, Transverse to Flow, ASTM E831
- Thermal Conductivity, ISO 22007-2, through-plane, 80*3mm discs
- Thermal Conductivity, ASTM E1461-07, through-plane, 10*10*3mm sample
- Thermal Conductivity, ASTM E1461-07, in-plane, ?25*0.4mm disc
- Thermal Conductivity, ISO 22007-2, in-plane, ?80*3mm discs
- Hot Ball Pressure Test, IEC 60695-10-2
- Deflection Temperature at 0.46 MPa (66 psi), ISO 75/Bf, Flatw 80*10*4 sp=64mm
- Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af, Flatw 80*10*4 sp=64mm
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
- UL RTI, Electrical, UL 746B
- UL RTI, Mechanical with Impact, UL 746B
- UL RTI, Mechanical without Impact, UL 746B
- Flammability, UL94, UL 94
- Glow Wire Test, IEC 60695-2-13
- Glow Wire Test, IEC 60695-2-13
- Glow Wire Test, IEC 60695-2-12
- Glow Wire Test, IEC 60695-2-12
- Zone 1
- Zone 2
- Zone 3
- Melt Temperature
- Mold Temperature
- Drying Temperature, Injection Molding
- Dry Time, Injection Molding
- Moisture Content
- Back Pressure
- Screw Speed
|
| | |