MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond EP76M-F Electrically Conductive, Two Part Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond EP76M-F is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing, and coating formulated to cure at room temperature or more rapidly at elevated temperatures. The outstanding feature of EP76M-F focuses on the faster set up time and full cure of the system when compared to the more standard EP76M. However, it should be noted that EP76M-F has a more limited open time. Unlike the majority of two part nickel conductive systems, EP76M-F has a one to one mix ratio by weight or volume and has no solvents or diluents. It has a paste consistency and is easy to apply. The volume resistivity of the cured system is 5-10 ohm-cm. EP76M-F is particularly noteworthy for its strength profile along with good resistance to chemicals including water, oil, and many acids and bases. EP76M-F has a wide temperature range of -60°F to +2 50°F. Adhesion to metals, composites, ceramics, glass, vulcanized rubbers and many plastics is excellent. Parts A and B are both colored gray. Master Bond EP76M-F is widely used in the electronic, electrical, computer and related industries where shielding and static dissipation are prime requirements, along with faster curing times.

Product Advantages:

  • Convenient mixing: one to one by weight or volume; contains no volatiles.
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly.
  • Versatile cure schedules; ambient temperature cures or fast elevated temperature cures as required.
  • Good electrical and thermal conductivity.
  • High bond strength to similar and dissimilar substrates.
  • Bonds well to a wide variety of substrates, especially metals and composites.
  • Faster set up and cure times.

Information provided by MasterBond®

Vendors:
Available Properties
  • Viscosity, Part A, thixotropic
  • Viscosity, Part B, thixotropic
  • Hardness, Shore D
  • Tensile Strength at Break
  • Shear Strength, Tensile lap, Al to Al
  • Volume Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Pot Life, 100 gram batch
  • Shelf Life, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.