Available Properties |
---|
- Density, ISO 1183/A
- Filler Content, Glass Fiber Reinforcement
- Water Absorption, ASTM D570
- Linear Mold Shrinkage, Flow, ASTM D955
- Linear Mold Shrinkage, Transverse, ASTM D955
- Tensile Strength, ASTM D638, Conditioned
- Tensile Strength, ASTM D638
- Tensile Strength, Yield, ISO 527-2, Conditioned
- Tensile Strength, Yield, ISO 527-2
- Tensile Strength, Yield, ISO 527-2, Conditioned
- Tensile Strength, Yield, ISO 527-2
- Tensile Strength, Yield, ISO 527-2, Conditioned
- Tensile Strength, Yield, ISO 527-2
- Tensile Strength, Yield, ISO 527-2
- Tensile Strength, Yield, ISO 527-2, Conditioned
- Elongation at Break, ASTM D638, Conditioned
- Elongation at Break, ASTM D638
- Elongation at Break, ISO 527-2
- Elongation at Break, ISO 527-2, Conditioned
- Elongation at Break, ISO 527-2, Conditioned
- Elongation at Break, ISO 527-2
- Elongation at Break, ISO 527-2
- Elongation at Break, ISO 527-2, Conditioned
- Elongation at Break, ISO 527-2
- Elongation at Break, ISO 527-2, Conditioned
- Tensile Modulus, ASTM D638, Conditioned
- Tensile Modulus, ASTM D638
- Tensile Modulus, ISO 527-2
- Tensile Modulus, ISO 527-2, Conditioned
- Tensile Modulus, ISO 527-2, Conditioned
- Tensile Modulus, ISO 527-2
- Tensile Modulus, ISO 527-2
- Tensile Modulus, ISO 527-2, Conditioned
- Tensile Modulus, ISO 527-2, Conditioned
- Tensile Modulus, ISO 527-2
- Flexural Strength, ASTM D790
- Flexural Strength, ASTM D790, Conditioned
- Flexural Strength, ISO 178
- Flexural Strength, ISO 178, Conditioned
- Flexural Strength, ISO 178, Conditioned
- Flexural Strength, ISO 178
- Flexural Strength, ISO 178
- Flexural Strength, ISO 178, Conditioned
- Flexural Strength, ISO 178, Conditioned
- Flexural Strength, ISO 178
- Flexural Modulus, ASTM D790
- Flexural Modulus, ASTM D790, Conditioned
- Flexural Modulus, ISO 178, Conditioned
- Flexural Modulus, ISO 178
- Flexural Modulus, ISO 178
- Flexural Modulus, ISO 178, Conditioned
- Flexural Modulus, ISO 178
- Flexural Modulus, ISO 178, Conditioned
- Flexural Modulus, ISO 178, Conditioned
- Flexural Modulus, ISO 178
- Compressive Strength, ASTM D695
- Shear Strength, ASTM D732, Conditioned
- Shear Strength, ASTM D732
- Izod Impact, Notched, ASTM D256, Conditioned
- Izod Impact, Notched, ASTM D256
- Izod Impact, Notched, ASTM D256
- Izod Impact, Notched (ISO), ISO 180/1A, Conditioned
- Izod Impact, Notched (ISO), ISO 180/1A
- Izod Impact, Unnotched (ISO), ISO 180/1U, Conditioned
- Izod Impact, Unnotched (ISO), ISO 180/1U
- Charpy Impact Unnotched, ISO 179/1eU
- Charpy Impact Unnotched, ISO 179/1eU, Conditioned
- Charpy Impact, Notched, ISO 179/1eA
- Charpy Impact, Notched, ISO 179/2eA, Conditioned
- Volume Resistivity, ASTM D257
- Surface Resistance, ASTM D257
- Dielectric Constant, ASTM D150
- Dielectric Constant, ASTM D150
- Dielectric Strength, ASTM D149
- Dissipation Factor, ASTM D150
- CTE, linear, Parallel to Flow, ASTM E831, TMA
- CTE, linear, Parallel to Flow, ASTM E831, TMA
- CTE, linear, Transverse to Flow, ASTM E831
- CTE, linear, Transverse to Flow, ASTM E831
- Melting Point, ASTM D3418, Peak
- Melting Point, ISO 11357-3, Conditioned
- Melting Point, ISO 11357-3
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/Af, Unannealed
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/Af, Unannealed, Conditioned
- Flammability, UL94, UL 94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
|
| | |