TPI is a thermoplastic polyimide film that has excellent, thermal, chemical, electrical and physical properties. With a continuous use temperature to 240°C (465°F), TPI films offer superior radiation resistance, excellent wear performance and resistance to chemicals. Key Attributes: Chemical Resistant; Flame Retardant; Good Electrical Properties; High Heat Resistance; Radiation (Gamma) Resistant Applications: Aircraft Applications; Automotive Applications; Electrical/Electronic Applications; Industrial Applications; Medical/Healthcare Applications; Oil/Gas Applications Standard Thicknesses and Widths - Widths are available from 22" (559 mm) to 56" (1422 mm). Products with widths <22 inches or >56 inches are available upon request. - Tolerances for widths are +/- 4mm. - For PI film, the standard thicknesses are 25 microns (1 mil) to 1016 microns (40 mil). Surface Finishes - Standard surface finish is P/M (polished / matte). - Custom finishes of P/P (polished / polished) and M/M (matte / matte) are available. Packaging - Film is supplied in a roll form of high quality, cardboard core of 3" (76mm) or 6" (152mm). - PVC cores are available upon request in 3" and 6" sizes. Information provided by Solvay Specialty Polymers. |