Hifax polypropylene resins based on the Catalloy process from LyondellBasell are used by customers in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable) and also automotive industries through both our resins and our well-known Hifax polypropylene compounds. Hifax is proven to provide customers with good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax 7430P SILHOUETTE GRAY a high flow, 1,300 MPa flexural modulus, UV-stabilized, paintable, unfilled thermoplastic elastomeric olefin (TEO). It provides excellent cold temperature ductility and very good surface appearance in mold in color applications. It is typically used for automotive exterior applications. Applications
Exterior Automotive Applications. |