MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Lord Adhesives CoolTherm™ EP-301 AD Epoxy Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LORD CoolTherm™ EP-301 AD resin is a general purpose epoxy resin designed for use with CoolTherm EP-6010 hardener to create a two-component system for applications requiring excellent heat transfer, high fluidity and good air release, such as potting intricate circuitry or encapsulating power devices.

Features: cures to a rigid system; provides good properties for room temperature cured system. suitable for use in castings up to 200g. offers dimensional stability over a temperature range from -65°C to +155°C. provides excellent high voltage insulation.

All information provided by Lord.

Vendors:
Available Properties
  • Specific Gravity
  • Water Absorption, cured
  • Viscosity
  • Linear Mold Shrinkage, cured
  • Hardness, Shore D, cured
  • Tensile Strength, cured
  • Elongation at Break, cured
  • Volume Resistivity, cured
  • Dielectric Constant, cured
  • Dielectric Strength, cured
  • Dissipation Factor, cured
  • CTE, linear, cured
  • Thermal Conductivity, cured
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, Mixed
  • Shelf Life, from date of manufacture when stored in original, unopened container
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.