Röchling GLASTHERM HT Insulation Sheet
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Glastherm Grade HT is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT is completely asbestos-free and is rugged to withstand rough handling during installation. Features of Grade HT include
  • High hot compressive strength
  • Low thermal conductivity
  • Oil and moisture resistant
  • Reduces heat loss
  • Helps control temperature
  • Faster mold startup
  • Information provided by Glastic Corporation

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.97 g/cc0.0712 lb/in³ASTM D-792
    Water Absorption 0.20 %0.20 %% by wt.; ASTM D-570
     
    Mechanical PropertiesMetricEnglishComments
    Flexural Strength 214 MPa31000 psiASTM D-790
    Compressive Strength  117 MPa
    @Temperature 288 °C
    17000 psi
    @Temperature 550 °F
    ASTM D-695
     124 MPa
    @Temperature 200 °C
    18000 psi
    @Temperature 392 °F
    ASTM D-695
     186 MPa
    @Temperature 150 °C
    27000 psi
    @Temperature 302 °F
    ASTM D-695
     338 MPa
    @Temperature 23.9 °C
    49000 psi
    @Temperature 75.0 °F
    ASTM D-695
    Compressive Modulus 12.4 GPa1800 ksiASTM D-695
    Izod Impact, Notched 4.27 J/cm8.00 ft-lb/inASTM D-256
     
    Electrical PropertiesMetricEnglishComments
    Dielectric Strength 2.00 kV/mm50.8 kV/inPerpendicular S/T in Air; ASTM D-149
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  22.1 µm/m-°C
    @Temperature 20.0 °C
    12.3 µin/in-°F
    @Temperature 68.0 °F
    Across Surface; ASTM D-696
     116.2 µm/m-°C
    @Temperature 20.0 °C
    64.56 µin/in-°F
    @Temperature 68.0 °F
    Across Thickness; ASTM D-696
    Thermal Conductivity 0.270 W/m-K1.87 BTU-in/hr-ft²-°FASTM C-177
    Maximum Service Temperature, Air 211 °C412 °F
     288 °C550 °F
    Flammability, UL94 HB
    @Thickness 23.9 mm
    HB
    @Thickness 0.940 in
     
    Descriptive Properties
    Standard ColorWhite/Green
    Thickness Tolerance in± 0.002

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.