Orbilan ORBILAN® PE 500 HMW-PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: Orbilan PE 500 plastic is used as cutting boards for the food industry and gastronomy, in refrigeration chambers as ram protection and for swing doors as well as at sports grounds for sheets or handrails when building ice-skating rinks.

Information provided by the manufacturer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183
Molecular Weight 500000 g/mol500000 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 868
Ball Indentation Hardness 50.0 MPa7250 psiISO 2039
Tensile Strength, Yield 27.0 MPa3920 psiISO 527-1
Elongation at Break >= 600 %>= 600 %ISO 527-1
Elongation at Yield 9.0 %9.0 %ISO 527-1
Modulus of Elasticity 1.20 GPa174 ksiISO 527-1
Charpy Impact, Notched 2.50 J/cm²11.9 ft-lb/in²ISO 179
Coefficient of Friction 0.200.20DIN 53 375
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmDIN 53 482
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 - 200 µm/m-°C
@Temperature 20.0 - 80.0 °C
83.3 - 111 µin/in-°F
@Temperature 68.0 - 176 °F
DIN 53 752-A
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 80.0 °C176 °Fcontinuous
Minimum Service Temperature, Air -60.0 °C-76.0 °Fcontinuous
 
Descriptive Properties
Attrition< 400Sand-Slurry procedure
Water Absorption< 0.01 mg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.