MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales
metalmen Is Your Direct to US Manufacturing Source for High Purity Metals

Aluminum, Al
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Pure Element

Material Notes: Aluminum is a silver-colored, low density (2.7 g/cc) metal that finds use in a huge variety of commercial applications. Unalloyed aluminum is ductile, exhibits moderate strength, and is very resistant to corrosion under most circumstances. Aluminum can be strengthened by the addition of appropriate alloying elements (Cu, Mg, Mn, Si, etc.) and subsequent heat/work treatments. Aluminum is commonly used in both wrought and cast forms.

The low density of aluminum results in its extensive use in the aerospace industry, and in other transportation fields. Its resistance to corrosion leads to its use in food and chemical handling (cookware, pressure vessels, etc.) and to architectural uses.

Over 1700 Aluminum alloy entries are listed in MatWeb, each with specific property data. Aluminum 1199 is the highest purity (99.99% Al min.) commercially available in structural form.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.6989 g/cc0.097504 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 26.9815426.9815426.981538 - 1995
Atomic Number 1313
Thermal Neutron Cross Section 0.215 barns/atom0.215 barns/atom
X-ray Absorption Edge 7.9511 Å7.9511 ÅK
 142.48 Å142.48 ÅLI
 172.16 Å172.16 ÅLII
 172.16 Å172.16 ÅLIII
Electrode Potential -1.69 V-1.69 V
Electronegativity 1.611.61Pauling
Ionic Radius 0.510 Å0.510 ÅCrystal Ionic Radius for Valence +3
Electrochemical Equivalent 0.3354 g/A/h0.3354 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 1515Annealed
Modulus of Elasticity 68.0 GPa9860 ksi
Poissons Ratio 0.360.36calculated
Shear Modulus 25.0 GPa3630 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000270 ohm-cm0.00000270 ohm-cm
Magnetic Susceptibility 6.0e-76.0e-7cgs/g
Critical Magnetic Field Strength, Oersted 101.9 - 107.9101.9 - 107.9
Critical Superconducting Temperature 1.73 - 1.77 K1.73 - 1.77 K
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 386.9 J/g166.4 BTU/lb
Heat of Vaporization 9462 J/g4071 BTU/lb
CTE, linear  24.0 µm/m-°C
@Temperature 20.0 - 100 °C
13.3 µin/in-°F
@Temperature 68.0 - 212 °F
 25.5 µm/m-°C
@Temperature 20.0 - 300 °C
14.2 µin/in-°F
@Temperature 68.0 - 572 °F
 27.4 µm/m-°C
@Temperature 20.0 - 500 °C
15.2 µin/in-°F
@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°F
Thermal Conductivity 210 W/m-K1460 BTU-in/hr-ft²-°F
Melting Point 660.37 °C1220.7 °F
Boiling Point 2519 °C4566 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.20 - 0.300.20 - 0.30strongly oxidized
 0.050
@Temperature 50.0 - 500 °C
0.050
@Temperature 122 - 932 °F
polished
Reflection Coefficient, Visible (0-1) 0.900.90tungsten light
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 100 %100 %
 
Descriptive Properties
CAS Number7429-90-5

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silver, Ag
Copper, Cu; Annealed
Iron, Fe
Titanium, Ti
Nickel, Ni

AMEAl00 / 3

Metalmen Sales
metalmen Is Your Direct to US Manufacturing Source for High Purity Metals

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.