System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Drill Down to All Materials Data Sheets
This series of pages is an inefficient set of links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
Replacing...
Polynt SMC 4200 R23 Sheet Molding Compound Good Pigmentability
Polynt SMC 4400 R12 Sheet Molding Compound
Polynt SMC 4500 R23 Sheet Molding Compound
Polynt SMC LP 2500 R25 Sheet Molding Compound
Polynt SMC LP 2500 R33 Sheet Molding Compound
Polynt SMC LP 6700 LW Sheet Molding Compound
Polynt SMC LPA 2000 R27 Sheet Molding Compound
Polynt SMC LPA 2000 R35 Sheet Molding Compound
Polynt SMC LPA 6703 LW NEUTRO Sheet Molding Compound
Polynt SMC LPMC 7000 LP Sheet Molding Compound
Polynt SMC LPMC 7200 Sheet Molding Compound
Polynt SMC LPMC 7300 RF Sheet Molding Compound
Polynt SMC LPMC 7680 Sheet Molding Compound
Polynt SMC LS 3000 R18 Sheet Molding Compound
Polynt SMC LS 3000 R33 Sheet Molding Compound
Polynt SMC LS 3022 R30 Sheet Molding Compound
Polynt SMC LS 3200 R20 C20 SMC, High Mechanical Properties
Polynt SMC LS 3200 R40 SMC, High Mechanical Properties
Polynt SMC LS 3300 R20 RF Sheet Molding Compound Fire Retardancy
Polynt SMC LS 3300 R25 RF Sheet Molding Compound Fire Retardancy
Polynt SMC LS 3600 R25 AE Sheet Molding Compound
Polynt SMC LS 3620 R35 AE Sheet Molding Compound High Fire Retardancy
Polynt SMC LS 3681 CL1 Sheet Molding Compound
Polynt SMC LS 3800 R25 RF C NERO Sheet Molding Compound
Polynt SMC S 8010 Sheet Molding Compound
Polynt SMC SF 12/25 RN-1090 Sheet Molding Compound
Polynt SMC VE 3700 Sheet Molding Compound
Polynt STYPOL® 040-4917 Acrylic Modified Gel Coat
Polynt STYPOL® 040-4950 Marble Clear Gel Coat
Polynt STYPOL® 040-4954 Marble Clear Gel Coat
Polynt STYPOL® 040-4956 Marble Clear Gel Coat
Polynt STYPOL® 040-4965 Marble Clear Gel Coat
Polynt STYPOL® 040-4985 Spray Granite Resin
Polynt STYPOL® 040-4988 Spray Granite Resin
Polynt STYPOL® 040-8003 Flame-Retardant RTM Resin
Polynt SUP 6000-1001 (1210) Sheet Molding Compound
Polynt Thermaclean® AQUAWASH® 095-0040 Solvent-Based Cleaner
Polynt Thermaclean® EP 095-0049 Solvent-Based Cleaner
Polynt Thermaclean® EXTRAFLUSH 095-0120 Solvent-Based Cleaner
Polynt Thermaclean® GUN FLUSH 095-0043 Solvent-Based Cleaner
Polynt Thermaclean® GUN FLUSH ES 095-0063 Solvent-Based Cleaner
Polynt Thermaclean® MARBLEWASH® 095-0113 Solvent-Based Cleaner
Polynt Thermaclean® REPLACETONE™ 095-0030 Water-Based Acetone Replacement Cleaner
Polynt Thermaclean® UNISOLVE™ EX 095-0102 Solvent-Based Cleaner
Polynt Thermaclean® UNIWIPE™ 095-0154 Water-Based Surface Cleaner
Polynt Thermaclean® Wipe-Bright® 095-0082 Water-Based Cleaner
Polynt V 322 HF Putty
Polynt V 422 RM Putty
Polyphosphazene Rubber (PZ, FZ)
Polyplastic Armamid® PA 6-1FR Nylon 6, Flame Retardant
Polyplastic Armamid® PA GF25-1FR Nylon 6, 25% Glass Fiber
Polyplastic Armamid® PA GF50-1 Nylon 6, 50% Glass Fiber
Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled
Polyplastic Armamid® PA6 GF 30-2HSM-902 Nylon, 30% Glass Filled
Polyplastic Armlen® PE MF 70-2FR Magnesium Hydroxide Filled Polyethylene
Polyplastic Armlen® PP 12IM-895 Impact Modified Polypropylene
Polyplastic Armlen® PP 3IM Impact Modified Polypropylene
Polyplastic Armlen® PP GF 20-1EX Polypropylene Copolymer, 20% Glass Fiber
Polyplastic Armlen® PP GF 30-1EX Polypropylene Copolymer, 30% Glass Fiber
Polyplastic Armlen® PP GF 30-5HS-901 Polypropylene, 30% Glass Filled
Polyplastic Armlen® PP GF MF 30-1 Polypropylene, 30% Glass and Mineral Filled
Polyplastic Armlen® PP MD 40-4HS-901 Polypropylene, 40% Mineral Filled
Polyplastic Armlen® PP MF 15-3 FR Polypropylene Homopolymer, Mineral Filled
Polyplastic Armlen® PP MF 20-2HS-901 Polypropylene, 20% Mineral Filled
Polyplastic Armlen® PP MF 20-3-901 Polypropylene, 20% Mineral Filled
Polyplastic Armlen® PP MF 20-3IM Impact Modified Polypropylene
Polyplastic Armlen® PP MF 25-3-901 Polypropylene, 20% Mineral Filled
Polyplastic Armlen® PP MF 30-3IM Polypropylene, 30% Mineral Filled
Polyplastic Armlen® PP MF 40-2HS Polypropylene, 40% Mineral Filled
Polyplastic Armlen® PP MF 40-3M Polypropylene Copolymer, 40% Calcium Carbonate
Polyplastic Armlen® PP MF 40-4M Polypropylene Copolymer, 40% Calcium Carbonate
Polyplastic Armlen® PP-10IM-901 Polypropylene, Mineral Filled
Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant
Polyplastic Armobond® PE 2K Polyethylene Adhesive Compound
Polyplastic Armoflen® PO MF 65-1 Linear Low Density Polyethylene, 65% Calcium Carbonate
Polyplastic Armoflen® PO MF 65-2 Linear Low Density Polyethylene, 65% Calcium Carbonate
Polyplastic Armoflen® PO MF 65-3 Polyethylene, 65% Mineral Filled
Polyplastic Armoflen® PO MF 65-4 Polypropylene, 65% Calcium Carbonate
Polyplastic Armoflen® PO MF 75-1 Polypropylene Homopolymer, 75% Calcium Carbonate
Polyplastic Armoflen® PO MF 75-2 Linear Low Density Polyethylene, 75% Calcium Carbonate
Polyplastic Compounds Armaloy® PC/ABS-1IM-9010 PC/ABS
Polyplastic Compounds Armamid® PA6 GF 15-1T Nylon 6, 15% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 15-1THSM Nylon 6, 15% Glass Fiber Reinforced, Heat Stabilized
Polyplastic Compounds Armamid® PA6 GF 20-1 Nylon 6, 20% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 20-3FR Nylon 6, 20% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 20-3FRM Nylon 6, 20% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 20-4FR Nylon 6, 20% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 20-5FRM Nylon 6, 20% Mineral Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 20-9FR Nylon 6, 20% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 25-1FR Nylon 6, 25% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 25-3FRAS Nylon 6, 25% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 30-1 Nylon 6, 30% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 30-1T Nylon 6, 30% Glass Fiber Reinforced, Impact Modified
Polyplastic Compounds Armamid® PA6 GF 30-1THSM Nylon 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyplastic Compounds Armamid® PA6 GF 30-2HS Nylon 6, 30% Glass Fiber Reinforced, Impact Modified
Polyplastic Compounds Armamid® PA6 GF 30-2HSM Nylon 6, 30% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 30-2TS-AF Nylon 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyplastic Compounds Armamid® PA6 GF 30-3M Nylon 6, 30% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 30-3MIM Nylon 6, 30% Glass Fiber Reinforced, Impact Modified
Polyplastic Compounds Armamid® PA6 GF 30-4T Nylon 6, 30% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 40-1LS Nylon 6, 40% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF 50-1 Nylon 6, 50% Glass Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF MiF 20-1 Nylon 6, 20% Glass/Mineral Fiber Reinforced
Polyplastic Compounds Armamid® PA6 GF MiF 30-2 Nylon 6, 30% Glass/Mineral Fiber Reinforced
Polyplastic Compounds Armamid® PA6 MF 15-1 Nylon 6, 15% Mineral Fiber Reinforced
Polyplastic Compounds Armamid® PA6 MF 15-2 Nylon 6, 15% Mineral Fiber Reinforced
Polyplastic Compounds Armamid® PA6 MiF 20-1FR Nylon 6, 20% Mineral Fiber Reinforced
Polyplastic Compounds Armamid® PA6-1FR Nylon 6, Heat-Stabilized
Polyplastic Compounds Armamid® PA6-1IM Nylon 6, Impact Modified
Polyplastic Compounds Armamid® PA6-2EX Nylon 6, Extrusion
Polyplastic Compounds Armamid® PA6-2T Nylon 6
Polyplastic Compounds Armamid® PA6-4FRX Nylon 6, Extrusion
Polyplastic Compounds Armamid® PA6-4T Nylon 6
Polyplastic Compounds Armamid® PA6-5FRX Nylon 6, Extrusion
Polyplastic Compounds Armamid® PA6-6EX Nylon 6, Extrusion
Polyplastic Compounds Armlen® PE-2AFX Polypropylene, Extrusion
Polyplastic Compounds Armlen® PO GF 25-1 Polypropylene, 25% Fiberglass Reinforced
Polyplastic Compounds Armlen® PO MD 70-2FRX Polypropylene, 70% Mineral Reinforced
Polyplastic Compounds Armlen® PP 11IM-9001 (black) Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP 17IM Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP 7IM-901 PP/PE
Polyplastic Compounds Armlen® PP E/P 15-1X Polypropylene, Extrusion
Polyplastic Compounds Armlen® PP E/P 15-2LS Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP E/P 15-3 Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP E/P 15-5MLS Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP E/P 15-6 (natural) Polypropylene Copolymer
Polyplastic Compounds Armlen® PP E/P 20-2 Polypropylene
Polyplastic Compounds Armlen® PP E/P 20-3 Polypropylene
Polyplastic Compounds Armlen® PP E/P 20-4MLS Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP E/P 20-5M Polypropylene
Polyplastic Compounds Armlen® PP GF 10-1HS Polypropylene, 10% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 10-2HS Polypropylene, 10% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 20-1EX Polypropylene, 20% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 20-1MEX Polypropylene, 20% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 20-2EX Polypropylene, 20% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 20-2LS Polypropylene, 20% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 25-1IM Polypropylene, 25% Glass Fiber Reinforced, Impact Modified
Polyplastic Compounds Armlen® PP GF 30-1EX Polypropylene, 30% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 30-2HS Polypropylene, 30% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 30-3 Polypropylene, 30% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 30-4HS Polypropylene, 30% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 30-5HS Polypropylene, 30% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 30-6HS-9010 (black) Polypropylene, 30% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 40-6HS-9010 (black) Polypropylene, 40% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP GF 50-6HS Polypropylene, 50% Glass Fiber Reinforced, Heat Stabilized
Polyplastic Compounds Armlen® PP GF MD 30-1 Polypropylene, 30% Glass Fiber Reinforced
Polyplastic Compounds Armlen® PP MD 10-1 Polypropylene, 10% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 10-2LS Polypropylene, 10% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 15-1FR Polypropylene, 15% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 20-1 Polypropylene, 20% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 40-11TS Polypropylene, 40% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 40-2TS Polypropylene, 40% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 40-3M Polypropylene, 40% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 40-4HS-901 (black) Polypropylene, 40% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 40-4M Polypropylene, 40% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 40-5TS Polypropylene, 40% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 40-5TS Polypropylene, 40% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 40-8.1TS Polypropylene, 40% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 45-10D Polypropylene, 45% Mineral Reinforced, Impact Modified
Polyplastic Compounds Armlen® PP MD 50-2TS Polypropylene, 50% Mineral Reinforced
Polyplastic Compounds Armlen® PP MD 50-5TS Polypropylene, 50% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 10-1FRX Polypropylene, 10% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 13-8IM Polypropylene, 10% Mineral Reinforced, Impact Modified
Polyplastic Compounds Armlen® PP MF 15-1FR Polypropylene, 15% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 15-3FR Polypropylene, 15% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 15-5IM-901 (black) Polypropylene, 15% Mineral Reinforced, Impact Modified
Polyplastic Compounds Armlen® PP MF 20-15IM Polypropylene, 20% Talc Filled
Polyplastic Compounds Armlen® PP MF 20-18IM (Natural) Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP MF 20-2 Polypropylene, 20% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 20-2HS Polypropylene, 20% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 20-3-901 (black) Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP MF 20-3IM Polypropylene, 20% Talc Filled
Polyplastic Compounds Armlen® PP MF 20-5IM Polypropylene, 20% Mineral Reinforced, Impact Modified
Polyplastic Compounds Armlen® PP MF 20-7IM Polypropylene, 20% Mineral Reinforced, Impact Modified
Polyplastic Compounds Armlen® PP MF 25-1 Polypropylene, 25% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 25-2TS Polypropylene, 25% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 25-3-901 (black) Polypropylene, 20% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 30-1 Polypropylene, 30% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 30-3IM Polypropylene, 30% Mineral Reinforced, Impact Modified
Polyplastic Compounds Armlen® PP MF 30-3TS Polypropylene, 30% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 30-4IM Polypropylene, 30% Mineral Reinforced, Impact Modified
Polyplastic Compounds Armlen® PP MF 35-1 Polypropylene, 35% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 40-1 Polypropylene, 40% Mineral Reinforced
Polyplastic Compounds Armlen® PP MF 40-2M Polypropylene, 40% Mineral Reinforced
Polyplastic Compounds Armlen® PP TPE 11-40D Polypropylene
Polyplastic Compounds Armlen® PP TPE-10-70A Polypropylene, Mineral Reinforced
Polyplastic Compounds Armlen® PP TPE-10-75A Polypropylene, Mineral Reinforced
Polyplastic Compounds Armlen® PP TPE-11-90A-9010 (black) Polypropylene
Polyplastic Compounds Armlen® PP TPE-17-J-80A Polypropylene, Mineral Reinforced
Polyplastic Compounds Armlen® PP-10IM-901 (black) Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP-12IM-8945 (alliance black) Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP-1EX Polypropylene
Polyplastic Compounds Armlen® PP-1FRX Polypropylene
Polyplastic Compounds Armlen® PP-2FR Polypropylene
Polyplastic Compounds Armlen® PP-2FRX Polypropylene
Polyplastic Compounds Armlen® PP-2IM Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP-3FRX Polypropylene
Polyplastic Compounds Armlen® PP-3IM Polypropylene, Impact Modified
Polyplastic Compounds Armlen® PP-4EX Polypropylene
Polyplastic Compounds Armlen® PP-4FRX Polypropylene
Polyplastic Compounds Armobond® PE-2X PE
Polyplastic Compounds Armoflen® PO MN 65-1 PP, Calcium carbonate Filled
Polyplastic Compounds Armoflen® PO MN 65-2 PP, Calcium carbonate Filled
Polyplastic Compounds Armoflen® PO MN 65-3 PP, Calcium carbonate Filled
Polyplastic Compounds Armoflen® PO MN 65-4 PP, Calcium carbonate Filled
Polyplastic Compounds Armoflen® PO MN 75-1 PP, Calcium carbonate Filled
Polyplastic Compounds Armoflen® PO MN 75-2 PP, Calcium carbonate Filled
Polyplastic Compounds Armoflen® PO MN 75-2 PP, Calcium carbonate Filled
Polyplastic Compounds Armoflen® PO MN 75-3 PP, Calcium carbonate Filled
Polyplastic Compounds Armoflen® PO MN 75-7 PP, Calcium carbonate Filled
Polyplastic Compounds Armoflen® PO MN 80-3 (natural) PP, Barium Sulphate Filled
Polyplastic Compounds Armoflen® PO MN 80-5 PP, Calcium carbonate Filled
Polyplastic Compounds Armoflen® PO MN 80-6 PP, Calcium carbonate Filled
Polyplastic Compounds Armoflen® PO MN 80-7 PP, Calcium carbonate Filled
Polyplastic Compounds Armovil® PPM-70A-901 Polyvinyl chloride
Polyplastic Compounds Technaset® A110 POM
Polyplastic Compounds Technaset® B110 POM
Polyplastic Compounds Technoloy® 2070 Polyvinyl chloride
Polyplastic Compounds Technotep® 30-1X-45D SEBS
Polyplastic Compounds Technotep® 35-1X-60A SEBS
Polyplastic Compounds Technoter® A-GF 30-?S PBT, 30% Glass Fiber Reinforced
Polyplastic Compounds Technoter® A-GF 30-FR PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polyplastic Compounds Tehnamid® AS-40-LTO Nylon 66, 40% Glass Fiber Reinforced
Polyplastic Compounds Tehnamid® A-SV25-ETK Nylon 66, 25% Glass Fiber Reinforced
Polyplastic Compounds Tehnamid® A-SV25-OD Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant
Polyplastic Compounds Tehnamid® A-SV-30-2TM Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyplastic Compounds Tehnamid® A-SV30-L Nylon 66, 30% Glass Fiber Reinforced
Polyplastic Compounds Tehnamid® A-SV30-LO Nylon 66, 30% Glass Fiber Reinforced
Polyplastic Compounds Tehnamid® A-SV30-LTO Nylon 66, 30% Glass Fiber Reinforced
Polyplastic Compounds Tehnamid® A-SV30-TAF Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyplastic Compounds Tehnamid® A-SV-35-2TM Nylon 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyplastic Compounds Tehnamid® A-SV-50-1 Nylon 66, 50% Glass Fiber Reinforced, Heat Stabilized
Polyplastic Compounds Torlen® PE-2X-901 HDPE
Polyplastic TechnoTep A® 65 A Thermoplastic Elastomer, Mineral Filled
Polyplastic TechnoTep B® 45 D Thermoplastic Elastomer, Mineral Filled
Polyplastic TechnoTep B® 60 A Thermoplastic Elastomer, Mineral Filled
Polyplastic TechnoTep B® 65 A Thermoplastic Elastomer, Mineral Filled
Polyplastic Torlen® PE 2K 901 High Density Polyethylene, Carbon Filled
Polyplastics Duracon® AW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding
Polyplastics Duracon® AW-01 CF2001/CD3501 Acetal Copolymer
Polyplastics Duracon® AW-01LV CF2001/CD3501 Acetal Copolymer
Polyplastics Duracon® AW-09 CF2001 Acetal Copolymer
Polyplastics Duracon® CH-10 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance
Polyplastics Duracon® CH-10 CD3501 Acetal Copolymer, CF
Polyplastics Duracon® CH-15 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance
Polyplastics Duracon® CH-15 CD3501 Acetal Copolymer, CF
Polyplastics Duracon® CH-20 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance
Polyplastics Duracon® CH-20 CD3501 Acetal Copolymer, CF
Polyplastics Duracon® CP-15X Acetal Co-polymer (POM), Creep resistant, Creep resistant
Polyplastics Duracon® CP15X CF2001 Acetal Copolymer
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.